Abstract
Related content
Lubrication behavior of Ni-Cr-based alloys containing MoS 2 at high temperature
By Dangsheng X.
Wear, Vol. 251, Iss. 1, 2001-10 ,pp. :
Lubrication of Mo, W, and their Alloys with H 2 S gas admixtures to room temperature air
Wear, Vol. 225, Iss. 1, 1999-04 ,pp. :
Treatment of MoS 2 films by high-energy heavy ion beams
Thin Solid Films, Vol. 277, Iss. 1, 1996-05 ,pp. :
Formation and characterization of self-lubricating MoS 2 precursor films on anodized aluminium
By Skeldon P. Wang H.W. Thompson G.E.
Wear, Vol. 206, Iss. 1, 1997-05 ,pp. :