Abstract
Related content
Wet abrasion and slurry erosion resistance of thermally sprayed oxide coatings
By Knuuttila J. Ahmaniemi S. Mantyla T.
Wear, Vol. 232, Iss. 2, 1999-10 ,pp. :
Cavitation erosion of flame spray weld coating of nickel-base alloy powder
Wear, Vol. 189, Iss. 1, 1995-10 ,pp. :
Erosion resistance of Ni-WC self-fluxing alloy coating at high temperature
Wear, Vol. 209, Iss. 1, 1997-08 ,pp. :