Author: Liu H. Sakamoto M. Nomura M. Ogi K.
Publisher: Elsevier
ISSN: 0043-1648
Source: Wear, Vol.250, Iss.1, 2001-10, pp. : 71-75
Disclaimer: Any content in publications that violate the sovereignty, the constitution or regulations of the PRC is not accepted or approved by CNPIEC.
Abstract
Related content
Effect of carbide orientation on abrasion of high Cr white cast iron
Wear, Vol. 189, Iss. 1, 1995-10 ,pp. :
Impact-abrasion behavior of low alloy white cast irons
Wear, Vol. 209, Iss. 1, 1997-08 ,pp. :
Tribological stability of Al 2 O 3 short fiber reinforced high Cr cast irons
By Sakamoto M. Liu H. Nomura M. Ogi K.
Wear, Vol. 251, Iss. 1, 2001-10 ,pp. :
Estimation of the Heat Stability of Hardened Cr-V Cast Irons
Materials Science Forum, Vol. 2016, Iss. 870, 2016-10 ,pp. :
Solidification and abrasion wear of white cast irons alloyed with 20% carbide forming elements
By Matsubara Y. Sasaguri N. Shimizu K. Yu S.a.K.
Wear, Vol. 250, Iss. 1, 2001-10 ,pp. :