Author: Shapkin P. Nasibov A. Vaksman Yu. Nitsuk Yu. Purtov Yu.
Publisher: MAIK Nauka/Interperiodica
ISSN: 0020-1685
Source: Inorganic Materials, Vol.42, Iss.8, 2006-08, pp. : 845-849
Disclaimer: Any content in publications that violate the sovereignty, the constitution or regulations of the PRC is not accepted or approved by CNPIEC.
Abstract
A process for indium doping of ZnSe single crystals during vapor phase growth is described. The solubility limit of indium in ZnSe is determined as a function of temperature and zinc selenide stoichiometry. The conclusion is drawn that the entire homogeneity range of ZnSe in the equilibrium phase diagram lies at selenium-enriched compositions.