Formation of protective anodic oxides on aluminium by low voltage anodising in sulphuric acid with cerium nitrate and tartaric acid additions

Author: Curioni M   Zuleta A A   Correa E   Pan X   Baron-Wiechec A   Skeldon P   Castaño J G   Echeverría F   Thompson G E  

Publisher: Maney Publishing

ISSN: 0020-2967

Source: Transactions of the Institute of Metal Finishing, Vol.90, Iss.6, 2012-11, pp. : 290-297