Improvement in the Tensile Bond Strength between 3Y-TZP Ceramic and Enamel by Surface Treatments

Author: Byeon Seon-Mi   Jang Yong-Seok   Lee Min-Ho   Bae Tae-Sung  

Publisher: MDPI

E-ISSN: 1996-1944|9|8|702-702

ISSN: 1996-1944

Source: Materials, Vol.9, Iss.8, 2016-08, pp. : 702-702