Abstract
Related content
Densification and Hydration of HMDSO Plasma Polymers
PLASMA PROCESSES AND POLYMERS (ELECTRONIC), Vol. 12, Iss. 1, 2015-01 ,pp. :
Phase diagrams for CVD diamond deposition from halogen-containing gas phase
By Liu Z.-J. Zhang D.W. Zhang J.-Y. Wan Y.-Z. Wang J.-T.
Thin Solid Films, Vol. 342, Iss. 1, 1999-03 ,pp. :